Year : 2018  |  Volume : 18  |  Issue : 5  |  Page : 21-22

OSC33: Correlation between applied occlusal load and force measured from dental prescale system


Date of Web Publication31-Oct-2018

Correspondence Address:
Login to access the Email id

Source of Support: None, Conflict of Interest: None


DOI: 10.4103/0972-4052.244624

Rights and Permissions

How to cite this article:
,. OSC33: Correlation between applied occlusal load and force measured from dental prescale system. J Indian Prosthodont Soc 2018;18, Suppl S1:21-2

How to cite this URL:
,. OSC33: Correlation between applied occlusal load and force measured from dental prescale system. J Indian Prosthodont Soc [serial online] 2018 [cited 2018 Nov 20];18, Suppl S1:21-2. Available from: http://www.j-ips.org/text.asp?2018/18/5/21/244624



Chen, Szu-Han, Chun-Ying Yu, Tong-Mei Wang, Tsung-Chieh Yang, Li-Deh Lin

School of Dentistry, National Taiwan University, Taipei, Taiwan

Aim: Dental Prescale System (DPS) was used to measure absolute occlusal load in previous studies. In DPS, a pressure-sensitive wax wafer, bitten by the patients, will change colour locally depending on the pressure levels exerted. The colour density was used to estimate occlusal forces. The aim of this study was to investigate the accuracy of Dental Prescale System in measuring occlusal load.

Materials and Methods: Compressive loads of 0.5, 1.0, 2.0 kgf were consecutively applied to a pair of opposing first molar teeth (D91S-200-MF, Nissin, Japan), which were mounted in maximal intercuspation, with the system pressure sheets (LLW, Fujifilm, Japan) interposed. The pressure sheets were later scanned. The total measured force (TMF), average measured pressure (AMP) and force at the most forceful area (P1) were analysed using pressure analysis software. ANOVA and linear regression were used for statistical analysis.

Results: The TMF measured by DPS at 0.5, 1.0, 2.0 kgf applied force were 1.073±0.206, 2.103±0.375, 4.573±0.212 kgf respectively; the AMP was 1.395±0.021, 1.540±0.049, 1.610±0.025 MPa and P1 was 0.845±0.253, 0.845±0.039, 0.988±0.041 MPa, respectively.

Conclusion: Although a positive correlation was observed between TMF and applied loads, the forces estimated from Prescale system was considerably larger than applied loads. A non-linearly relation was observed between applied loads and both AMP and P1.






 

Top
 
 
  Search
 
Similar in PUBMED
   Search Pubmed for
   Search in Google Scholar for
Access Statistics
Email Alert *
Add to My List *
* Registration required (free)

 
  In this article

 Article Access Statistics
    Viewed30    
    Printed0    
    Emailed0    
    PDF Downloaded13    
    Comments [Add]    

Recommend this journal


[TAG2]
[TAG3]
[TAG4]